To recipes helpdesk

Question

Posted on: March 6 2013

My bath oil on the basis of Eumulgin is no longer clear. Comperlan KD (coconut fatty acid-dithanolamide) 50ml Miglyol B 812 (medium chain triglyceride) 200ml Eumulgin

1000 NI (macrogol cetyl/Oleyl ether) 50ml
Cetiol V (decyloleate) 50ml
liquid paraffin AD 500ml < BR/> Normally I get provided heating a bright bath oil. Lately, coagulation occurs after cooling and the oil becomes cloudy and more viscous. Can this be due to the Macrogol cetyl/Oleyl ether lying down?

Answer

I suspect that instead of Eumulgin 1000 NI you should use Eumulgin O 5. The intervention by the RIZIV in the cost of this preparation is void by the use of this product. Alternatives are on the website. If my proposal does not offer any satisfaction, I suggest you to focus on following composition:
R/Cetiol V 50ml
Eumulgin O5 75ml
Comperlan KD 25ml
Paraffin Oil 50 ml

total 200 ml

even better: Comperlan K replacement by Comperlan OD.